Process
Two chemicals, sunlight and water. How every print in this site is made by hand.

Step 1 of 6
Mix
Ferric ammonium citrate and potassium ferricyanide, equal parts, mixed in dim light.
Step 2 of 6
Coat
Brushed onto cotton rag paper in two passes, then dried in a dark drawer overnight.
Step 3 of 6
Expose
A digital negative is pressed against the paper under glass and left in the sun for 8 to 20 minutes.
Step 4 of 6
Wash
Running water clears the unexposed chemistry. The yellow-green turns to blue in seconds.
Step 5 of 6
Tone
Some prints are toned in tea or tannin to warm the blacks and shift the blues to slate.
Step 6 of 6
Dry & sign
Flattened under weight for two days, then signed, numbered and stamped on the back.